S 275 J0 is a non-alloy structural steel with a carbon content below 0.2% that is commonly used for structural and construction applications in Norway. Its chemical composition includes a minimum of 0.18% carbon and a maximum of 1.5% manganese, 0.04% phosphorus, 0.04% sulfur, and 0.009% nitrogen. It is referenced in several standards including NS EN 10025 for hot rolled steel products in Norway.
S 275 J0 is a non-alloy structural steel with a carbon content below 0.2% that is commonly used for structural and construction applications in Norway. Its chemical composition includes a minimum of 0.18% carbon and a maximum of 1.5% manganese, 0.04% phosphorus, 0.04% sulfur, and 0.009% nitrogen. It is referenced in several standards including NS EN 10025 for hot rolled steel products in Norway.
Direitos autorais:
Attribution Non-Commercial (BY-NC)
Formatos disponíveis
Baixe no formato PDF, TXT ou leia online no Scribd
S 275 J0 is a non-alloy structural steel with a carbon content below 0.2% that is commonly used for structural and construction applications in Norway. Its chemical composition includes a minimum of 0.18% carbon and a maximum of 1.5% manganese, 0.04% phosphorus, 0.04% sulfur, and 0.009% nitrogen. It is referenced in several standards including NS EN 10025 for hot rolled steel products in Norway.
Direitos autorais:
Attribution Non-Commercial (BY-NC)
Formatos disponíveis
Baixe no formato PDF, TXT ou leia online no Scribd
Structural and constructional steels NS EN 10025(1994) Non-alloy, quality steel; Hot rolled products of non-alloy structural steels
Chemical Composition [%]
Criterion C Mn P S N Min Max 0.1800 1.5000 0.0400 0.0400 0.0090 Approx -
- C C content <= 0,20 for t >= 150 mm
Cross Reference Table
Material S 275 J 0 A 572 Grade 42 43 C S275JO / Fe 430 C S 275 J 0 S 275 J 0 S 275 J 0 1.0143 Standard AFNOR NF ASTM B.S. DIN NBN UNE UNI WN Country France USA United Kingdom Germany Belgium Spain Italy Germany