Você está na página 1de 2

1 AS 2891.12.

1—1995

Australian Standard
Methods of sampling and testing asphalt

Method 12.1: Determination of the permanent


compressive strain characteristics of asphalt—
Dynamic creep test

1 SCOPE This Standard sets out the method for determining, at standard test conditions, the
This is a free 1 page sample. Access the full version at http://infostore.saiglobal.com.

accumulated axial deformation response of asphalt mixtures normally used in pavements. The
method may be used for cores sampled from the roadway, or for specimens compacted in the
laboratory.

2 REFERENCED DOCUMENTS The following documents are referred to in this Standard:

AS
1545 Methods for the calibration and grading of extensometers
2193 Method for calibration and grading of force-measuring systems of testing machines
2891 Methods of sampling and testing asphalt
2891.1 Method 1: Sampling of asphalt
2891.2.2 Method 2.2: Sample preparation—Compaction of asphalt test specimens using a
gyratory compactor
2891.8 Method 8: Voids and density relationships for compacted asphalt mixes
2891.9.2 Method 9.2: Determination of bulk density of compacted asphalt—Presaturation
method
3 DEFINITION For the purpose of this Standard, the definition below applies:
3.1 Accumulated strain—the accumulation of strain within a material when it is subjected to
cyclic loading.

4 APPARATUS The following apparatus is required:


(a) Testing machine —a pneumatic or hydraulic testing machine, capable of applying a
rectangular shaped load pulse through a hemispherically ended loading ram for 0.5 ±0.05 s
hold time with a peak load equivalent to applied compressive stress of 200 ±5 kPa
(see Note 1), and of then removing the load and resting for a period of 1.5 ±0.05 s before
application of the next load pulse.
The testing machine shall contain two circular, steel platens. One platen shall be able to
pivot on the hemispherical end of the loading ram, and the other platen shall be located
centrally on the axis of the machine. The diameters of the platens shall be greater than the
diameter of the test specimen. The thickness of the platens shall be about 25 mm.
The platens shall be of hardened steel, essentially smooth and free from scratches. The
finish of the platens shall be consistent with that obtained by lapping with P600 grit silicon
carbide paper. The distance between the platens shall be adjustable over the range 40 mm
to 200 mm (see Note 2).

COPYRIGHT
This is a free preview. Purchase the entire publication at the link below:

AS 2891.12.1-1995, Methods of sampling and


testing asphalt Determination of the permanent
compressive strain characteristics of asphalt -
This is a free 1 page sample. Access the full version at http://infostore.saiglobal.com.

Dynamic creep test

Looking for additional Standards? Visit SAI Global Infostore


Subscribe to our Free Newsletters about Australian Standards® in Legislation; ISO, IEC, BSI and more
Do you need to Manage Standards Collections Online?
Learn about LexConnect, All Jurisdictions, Standards referenced in Australian legislation
Do you want to know when a Standard has changed?
Want to become an SAI Global Standards Sales Affiliate?

Learn about other SAI Global Services:

LOGICOM Military Parts and Supplier Database


Metals Infobase Database of Metal Grades, Standards and Manufacturers
Materials Infobase Database of Materials, Standards and Suppliers
Database of European Law, CELEX and Court Decisions

Need to speak with a Customer Service Representative - Contact Us

Você também pode gostar